1. … Due to the complex carbide combination of Cobalt, Chromium, Aluminium, Zirconium and a extreme high Tungsten content the wear resistance …
  2. … alloy for welding aluminium-magnesium based alloys with maximum 5% Mg. Zirconium added as grain refiner to improve both the bending and … EN AW 5086, EN AW 6060, EN AW 6005A, EN AW , EN AW 6061, EN AW 7020, EN AW 7021, EN AC 51400, EN AC 51300, EN AC 51100, EN AW 5454 … AlMg 4.5MnZr …
  3. … alloy for welding aluminium-magnesium basis alloys with maximum 5% Mg. Zirconium acts as grain-refiner to improve both the bending and the … EN AW 5086, EN AW 6060, EN AW 6005A, EN AW , EN AW 6061, EN AW 7020, EN AW 7021, EN AC 51400, EN AC 51300, EN AC 51100, EN AW 5454 … AlMg 4.5MnZr …
  4. Brand: UTP
    CEWELD Product: AA NiCro 600
    BÖHLER NIBAS 70/20 Mn-FD … 55 … FOXcore Nicro 83-TO …
  5. … Spec. 5 L: Grade A, B, X42, X 46, X 52, X 56, X 60, (Root X 70) … E 7028 … A 5.1: E 7028 … 2560-A: E 42 2 B 83 …
  6. Brand: Böhler Welding
    CEWELD Product: AA NiCro 600
    FOXcore Nicro 83-T0 … 235 … NIBAS 70/20 Mn-FD …
  7. … CEWELD E 7024 (150) is a high performance electrode with a thick rutile coating … electrode can be used for all kinds of steel constructions. CEWELD E 7024 (150) has a high current carrying capacity and good striking … 70; A 633, Gr. A, C; A 711 Gr. 1013;  API 5 L Gr. B, X42, X52    … E 7024 (150) … A 5.1: E 7024 … 2560-A: E 42 0 RR 73 …
  8. … CEWELD E 7027 is a high performance electrode with a thick coating and a … and offers excellent impact properties down to -40°C. CEWELD E 7027 has a high current carrying capacity and self detaching porous … Spec. 5 L: Grade A, B, X42, X 46, X 52, X 56, X 60, (Root X 70) … E 7027 … A 5.1: E 7027 … 2560-A: E 42 2 RA 73 …
  9. … CEWELD E 7024 (200) is a high performance electrode with a thick rutile coating … electrode can be used for all kinds of steel constructions. CEWELD E 7024 (200) has a high current carrying capacity and good striking … 65, 70; A 633, Gr. A, C; A 711 Gr. 1013;  API 5 L Gr. B, X42, X52  … E 7024 (200) … A 5.1: E 7024 … 2560-A: E 42 0 RR 73 …
  10. Zirconium often is chosen for its resistance to corrosion from most … should not be more than -60 degrees F (-51 degrees C). … Welding Zirconium alloys in general but also for successfully weld zirconium to titanium, tantalum, niobium (columbium) and vanadium … will be stringer and less ductile than the base metals. … Zirconium Zr 702 … A 5.24: ERZr2 …