1. … Replaceable polyurethane tyres are mounted onto a cast steel drumdor durability and siperior traction. … Euroweld - RedRock Column & Boom …
  2. … helium are used as shielding gases in TIG welding to prevent oxidation during the welding process. A well-maintained and properly adjusted …
  3. … good hardness in the first layer. A buffer layer with OA 4370 or OA MnCr is recommended in case of sensible base material or old …
  4. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast …
  5. … or 2 layers should not be deposited. A Buffer layer with OA 4370 or OA MnCr is recommended in case of old layers or critical base metals.. … …
  6. … that this steel is distinctly vulnerable to sensitization phenomenon during welding, even though martensite hogs a great amount of carbon …
  7. … old layers. Weldable without protective gas.Corresponding electrode: Dur 62 S … 64-68 HRc hardfacing alloy, Cement, Mineral mixing, hammers, …
  8. … alloy containing Nickel for more strength and bridging capability during brazing with excellent rebuilding properties.  Flux/Paste: …
  9. … to cut the wreck into liftable pieces. find out more about CEWELD DUR CS … sawing shipwrecks with tungsten brazing parts …
  10. … MPa and some wires only have 600 MPa but why is this so important? During wire feeding through the welding gun the wire surface is …