- … Excellent welding properties and mechanical strength up to 460 MPa yield …
- … Very good welding and wetting characteristics and high resistance to cracks and …
- … and low temperature fine grained structural steels. Excellent welding properties in combination with FL 155 high basic flux even in … kJ/cm and interpass temperature between 100 and 150ºC. … Reh < 690 MPa Iso 15608: 2.2 u 3.2 ( 460 < Reh ≤ 690(700) MPa ) 1.8914, 1.8927, …
- … is good machinable. Very good weld deposit appearance and outstanding welding properties on both AC and DC+. Preheating is not required. …
- … an agglomerated semi-basic low hydrogen SAW flux. Basicity: about 1,7 (according to Boniszewski) Current: DC or AC, in single or multi-wires …
- … treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11, G-AlSi12 (Cu), G-AlSi7Mg, G-AlSi6Cu4, …
- … Extreme easy to weld with excellent welding properties. Suitable to offer creep resistance for working temperatures up to 550º Celsius. … Typ 1Cr0,5Mo, ISO 15608: ~5,1 1.7335, 1.7262, 1.7728, 1.7218, …
- … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni … relatively severe thermic shock, and is superior to type 309L. … ISO 15608: 8.1 Austenit ≤ 19 % Cr , TÜV 1000: Gr. 21-30, Type: 25% …
- … Rutile stick electrode for welding of steam production plants, steam pipes and similar joints made … quenched and tempered for cementation and nitrating. … Typ 1Cr 0,5Mo, ISO 15608: ~5,1 1.7335, 1.7262, 1.7728, 1.7218, …
- … grained structural steels up to 460 MPa yield strength. Excellent welding properties in combination with FL 155 high basic flux even in …