- … Tempered 560° C ~ 52 HRc Tempered 450° C ~ 49 HRc Tempered 350° C ~ 48 HRc Soft annealed 250 HB … 45-52 HRc 1.2567, 1.2365, …
- … resistance to intercrystallin corrosion and wet corrosion up to 350°C (662 °F). Corrosion-resistance is similar to low-carbon CrNiMo …
- … it is necessary to buffer with an electrode like CEWELD E DUR 350 Kb / E 11018-G that delivers a welding deposit of less hardness. …
- … and leaves a fine rippled shiny surface. Max. service temperature 350ºC. Corrosion resistance similar to low carbon CrNiMo(Mn,N)-steels. …
- … layers it is necessary to buffer with an electrode like CEWELD® E DUR 350 Kb that delivers a welding deposit of less hardness. Overlays on …
- … resistance to intercrystallin corrosion and wet corrosion up to 350°C (662 °F). Corrosion-resistance is similar to low-carbon CrNiMo …
- … for stabilized and non-stabilized CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down to -196°C. Good resistance to … ISO 15608: 8.1 Austenit ≤ 19 % Cr 9%Ni ,TÜV 1000: Gr. 21 - 22 (29 max.350°C), 1.4301, 1,4306, 1.4307, 1.4308, 1.4311, 1.4312, 1.6900, 1.6901, …
- … 625 TÜV S2 TÜV S3Si TÜV S3Si-FL155 T ÜV S2Mo TÜV S3NiMo1 TÜV SACW 690 T Ü V 6013S TÜV 6013T TÜV 7016 TÜV 7018-1 TÜV 7018-A1 …
- … resistance to intercrystalline corrosion and wet corrosion up to 350°C (662 °F). Corrosion-resistance is similar to low-carbon …
- … up to much higher temperatures. Preheating is recommended at 150 - 350° C. depending on the thickness of the base metal. Similar base …